Project case study

Creating a Stunning 31’ Cedar Fence with Top Trim for Nathaniel Cameron in Pasadena, TX

Nathaniel Cameron wanted a 31-foot cedar privacy fence with a 2×12 top trim, finished with a protective stain. Here is that job in photos, plus what the USDA Wood Handbook says about why cedar should be finished soon after it goes up.

  • Reviewed Oct 29, 2026
  • Source: USDA Wood Handbook Ch.16
  • 2 job photos
Cedar privacy fence beside a two-storey house
The finished 31-foot cedar privacy fence with a 2×12 top trim.
The short answer

Nathaniel Cameron’s 31-foot cedar privacy fence was built with a 2×12 top trim and finished with a protective stain. That stain matters more than it might look: USDA Forest Products Laboratory research found that how soon a cedar surface gets finished after installation strongly affects how long that finish lasts.

31 ftLength of Nathaniel Cameron’s cedar privacy fence
2×12Dimension of the top trim board running the length of the fence
StainedA protective stain was applied to the cedar after installation
3 vs. 13 yrsPaint life in one Wood Handbook test: boards exposed 16 weeks before finishing vs. just 1 week

Source: USDA Forest Products Laboratory, Wood Handbook FPL-GTR-282 (2021), Ch.16.

The job: a 31-foot cedar fence with a 2×12 top trim

Nathaniel Cameron wanted a 31-foot cedar privacy fence with a 2×12 top trim running the length of it. Cedar was chosen for its natural resistance to rot and insects, the posts were set deep and secure in the ground, and the fence was finished with a protective stain.

The photos below are from that job.

Wood privacy fence running beside a pale blue house with a white porch
The cedar privacy fence running beside the house.

What happens to cedar if it never gets finished

Cedar is naturally resistant to decay and insects, but an unfinished surface still changes with years of sun and rain. USDA Forest Products Laboratory testing measured that change directly, tracking how many micrometers of surface wood erode away over time on unfinished boards exposed outdoors, facing south. Earlywood — the softer growth rings laid down early in a tree’s growing season — erodes noticeably faster than the denser latewood next to it, which is part of why bare, weathered wood develops that rougher, silvery-grey look over the years.

Bar chart of erosion in micrometers for unfinished western redcedar at 4, 8 and 16 years, each year showing a shorter latewood bar next to a taller earlywood bar. Latewood (LW) — denser growth rings, erodes slower Earlywood (EW) — softer growth rings, erodes faster 200 LW 500 EW4 YEARS 595 LW 1090 EW8 YEARS 1380 LW 1945 EW16 YEARS Left unfinished: how much a cedar surface erodes, in micrometers Western redcedar, SG 0.31, vertical surface facing south, no finish. Earlywood erodes roughly 2-3x faster than latewood at every point measured.
S-1
DrawingErosion of unfinished cedar, earlywood vs. latewood
BasisUSDA Forest Products Laboratory, Wood Handbook FPL-GTR-282 (2021), Table 16-1 (western redcedar, SG 0.31, vertical south-facing exposure, no finish)
ScaleNot to scale
At every point measured, earlywood (the softer growth rings) eroded about 2-3x faster than latewood on unfinished cedar.

Why timing matters: the Wood Handbook’s “sunburn” finding

A separate Wood Handbook section, titled Sunburn — UV Exposure and Paint Adhesion, explains why Mustang finishes cedar promptly rather than letting a new fence weather first: “Research has shown that surface degradation of wood facing south for as little as one week prior to painting significantly shortened the service life of paint.” In the cited experiment — vertical-grain western redcedar with a primer and two coats of latex topcoat — panels that were primed and painted with no prior sun exposure were still in good condition after 20 years. Panels that sat in the sun for just 1 week before finishing began peeling around 13 years. Panels left exposed for 16 weeks needed refinishing within 3 years. The Handbook’s advice for low-density species like cedar: “finish the wood as soon as possible after installation, or better yet, prime it before installation.”

Bar chart showing three groups: 0 weeks of sun exposure before finishing lasted 20-plus years in good condition, 1 week lasted 13 years before peeling, and 16 weeks needed refinishing within 3 years. 20+ yrs, still good 13 yrs to peeling 3 yrs, refinish needed 0 WEEKS1 WEEK16 WEEKS Sun exposure before finishing vs. how long the paint lasted One Wood Handbook experiment, vertical-grain western redcedar, primer + 2 latex topcoats. Longer unprotected sun exposure before finishing shortened paint life.
S-2
DrawingPre-finish sun exposure vs. years before repainting
BasisUSDA Forest Products Laboratory, Wood Handbook FPL-GTR-282 (2021), Ch.16 (“Sunburn — UV Exposure and Paint Adhesion”)
ScaleNot to scale
The longer a board sat in the sun before being finished, the sooner its paint failed, in this one Wood Handbook test.

How a crew checks for “sunburned” wood

The Wood Handbook also describes a simple field check: stick a strongly adhering piece of tape to the wood, press it on well, and snap it off quickly. If loose surface wood fibers come off stuck to the tape, those fibers were never going to hold a film-forming finish either — the same way they just came off the tape, they would eventually let the paint peel off, too. The Handbook adds a visual tell: “If wood looks weathered and silver or grey, it is severely sunburned.”

Two boards side by side with a strip of tape applied at an angle. On the left, finished promptly, the tape lifts clean. On the right, sunburned from weathering first, small wood fibers come off stuck to the tape. TAPE LIFTS CLEANFINISHED PROMPTLYsurface fibers stay intact TAPE PULLS UP WOODSUNBURNED (weathered first)loose fibers come off with the tape The tape test: is this board sunburned? Wood Handbook Ch.16: stick strongly-adhering tape to the wood and snap it off. If wood fibers come off with the tape, the surface is sunburned and a film-forming finish will peel the same way.
S-3
DrawingThe tape test for sunburned wood
BasisUSDA Forest Products Laboratory, Wood Handbook FPL-GTR-282 (2021), Ch.16 (tape test for sunburned wood before finishing)
ScaleNot to scale
Wood finished before it sunburns keeps its surface fibers intact; weathered wood sheds them, tape or paint alike.

Cedar finish-timing check

Pick how long a cedar surface sat in the sun before it was primed or stained. Based on one USDA Forest Products Laboratory test. General guidance, not a guarantee for your project.

What the test found

USDA Forest Products Laboratory, Wood Handbook FPL-GTR-282 (2021), Ch.16: vertical-grain western redcedar, primer + 2 latex topcoats. No prior sun exposure: still in good condition after 20 years. 1 week of exposure first: paint began peeling at 13 years. 16 weeks of exposure first: refinishing was needed within 3 years.

What Google reviewers say about Mustang Fencing

5.0
91 Google reviews · read them all on Google
★★★★★
My new fence looks fantastic and has added both privacy and style to my yard. Highly recommend their services for anyone in need of fencing!
Jaweria Malik · Google review · 2 years ago
★★★★★
I like their quality, and at this price, it is a great deal to acquire a fence. Overall, I like their competent service. Would book them again if necessary.
Shoaib Saleem · Google review · a year ago
★★★★★
A family friend recommends this company to me they were very fast, reliable, and cost officiant! I highly recommend them for the best fencing company ever!
Valerie Whitener · Google review · a year ago

Reviews shown word for word from the Mustang Fencing Services Google Business Profile (Galveston), captured 2026-10-26.

Questions we get about this

What size is the top trim on Nathaniel Cameron’s fence?
A 2×12 board running the length of the fence, on top of the cedar privacy pickets.
Why was Nathaniel Cameron’s cedar fence finished with a protective stain?
USDA Forest Products Laboratory research found that cedar left exposed to sun before finishing loses paint-adhesion performance quickly; finishing promptly (or priming before installation) gets much longer service life out of the finish.
What happens to cedar if it is never finished?
USDA testing measured the surface eroding away over the years outdoors, with the softer earlywood growth rings eroding roughly 2-3x faster than the denser latewood — part of why bare, weathered cedar turns a rougher, silvery-grey.
How do you tell if a board is "sunburned" from sitting in the sun too long before finishing?
The Wood Handbook describes pressing strongly adhering tape onto the wood and snapping it off. If loose wood fibers come off with the tape, the surface is sunburned. Wood that looks weathered and silver or grey is a visual sign of the same thing.
Does finishing timing really change how long paint or stain lasts?
In one Wood Handbook test on western redcedar, boards finished with no prior sun exposure stayed in good condition past 20 years; boards exposed just 1 week first started peeling around 13 years; boards exposed 16 weeks first needed refinishing within 3 years.

Sources

Checked October 29, 2026. Rules change, so confirm with the City before you build.

  1. USDA Forest Products Laboratory, Wood Handbook FPL-GTR-282 (2021), Chapter 16: Finishing of Wood — Table 16-1 (erosion of unfinished wood over years, earlywood vs. latewood); the “Sunburn — UV Exposure and Paint Adhesion” section (pre-finish sun exposure vs. paint service life, and the tape test for sunburned wood).
Free on-site estimate

Planning a wood fence or gate?

We’ll walk the property, talk through wood choice, trim and finishing, and put it on a written quote.

Page reviewed October 29, 2026 by Mustang Fencing Services, Galveston. Next review due April 2027.